Steel

  • Density 7800 kg/m3


Stainless steel

Property Units Typical Type 316 Type 316L
Ultimate Tensile Strength [N/mm^2] 586 517.1 min 482.6 min
0.2% Offset Yield Strength [N/mm^2] 303.37 206.84 min 172.37 min
Elongation in 2 inches [%] 56 40 min 40 min
Reduction in Area [%] 69
Hardness, Rockwell [B] 81 95 max 95 max
Density [Kg/m^3] 7 888.77
Modulus of Elasticity [psi] 29 x 10^6
  • Quality 304 (A2) and 316/316L (A4) are suitable for use on board.


Aluminum

  • Density 2700 kg/m3
  • 5083-H111 can be bended without restrictions
  • 5083-H321 limited bending (no hard bigger than 45 degrees)


Diesel

  • Density 850 kg/m3


Gasoline

  • Density 720 kg/m3

Carbon steel diamond plate

Th Diamond plate Normal plate Diamond % heavier
mm Kg/m^2 Kg/m^2
3 26.17 23.40 10.6%
4 34.91 31.20 10.6%
4.5 36.91 35.10 4.9%
5 43.60 39.00 10.5%
6 48.68 46.80 3.9%
8 64.40 62.40 3.1%
10 80.12 78.00 2.6%
12.5 99.70 97.50 2.2%
  • Quality 304 (A2) and 316/316L (A4) are suitable for use on board.